ACID
RESISTANT MORTAR (IS 4832 - Part I) |
|
Property |
Sodium
Silicate Type |
Potassium
Siliate Type |
|
Working time
(minutes) min. at 27±2șC |
15 |
20 |
|
Flexural
Strength (kg/cm2) min. at 7 days |
35 |
40 |
|
Compressive
Strength (kg/cm2 min. at 7 days |
100 |
150 |
|
Bond
Strength (kg/cm2) min. |
5 |
|
Absorption
of Toluene (% by weight) max. |
18 |