| ACID RESISTANT MORTAR (IS 4832 - Part I) |
|
|
Property |
Sodium
Silicate Type |
Potassium
Silicate Type |
|
Working time (minutes) min. at 27±2ºC |
15 |
20 |
|
Flexural Strength (kg/cm2) min. at 7 days |
35 |
40 |
| Compressive Strength (kg/cm2) min. at 7 days |
100 |
150 |
| Bond Strength (kg/cm2) min. |
5 |
| Absorption of Toluene (% by weight) max. |
18 |